DAPZOI
Home Topics Quiz Login


Forging Defects MCQ Questions & Answers

Forging Defects MCQs : This section focuses on the "Forging Defects". These Multiple Choice Questions (MCQs) should be practiced to improve the Forging Defects skills required for various interviews (campus interview, walk-in interview, company interview), placement, entrance exam and other competitive examinations.




Question 1

For closed die forging which of the following hammer suits best?

A. Drop hammer
B. HERF
C. Power hammer
D. Blow hammer

View Answer

Question 2

If the spread ratio coefficient of the particular metal under forging is 0, this indicates that _____

A. all the energy is gone in elongation
B. all the energy has gone in spread the width
C. the thickness of the material reached zero
D. the thickness of the material remains unchanged

View Answer

Question 3

If the spread ratio coefficient of the particular metal under forging is 1, this indicates that _____

A. all the energy is gone in elongation
B. all the energy went in spread the width
C. the thickness of the material reached zero
D. the thickness of the material remains unchanged

View Answer

Question 4

The coefficient of spread is not given by which mathematical expression?

A. S=Width elongation/ Thickness contraction
B. S=ln(w1/wo)/ln(ho/h1)
C. S=1-[length elongation/ thickness contraction]
D. S=length elongation/thickness contraction

View Answer

Question 5

The cogging is related to which of the following metal working/forging operation?

A. Open die forging
B. Closed die forging
C. Press forging
D. Impact forging

View Answer

Question 6

The concave die is effective in reducing the secondary tensile stress in the material and also to avoid the central cracking.

A. True
B. False

View Answer

Question 7

The counterblow hammer is competent solution to reduce the problem of ground shock and noise while using the forging hammer.

A. True
B. False

View Answer

Question 8

The flaking of forged material is due to the presence of which of the following element?

A. Oxygen
B. Hydrogen
C. Sulfur
D. Nitrogen

View Answer

Question 9

The large-sized hot forging material is cooled very slowly after working.

A. True
B. False

View Answer

Question 10

Which is the primary element to cause the hot shortness in the metal?

A. Oxygen
B. Carbon
C. Sulfur
D. Nitrogen

View Answer

Question 11

Which of the following forging hammer has the highest velocity on impact?

A. Gravity drop hammer
B. Power drop hammer
C. Hydraulic press
D. HERF

View Answer

Question 12

Which of the following forging hammer has the lowest velocity of impact?

A. Gravity drop hammer
B. Power drop hammer
C. Hydraulic press
D. HERF

View Answer